ПредпросмотрISO 5754 specifies the dimensions of an unnotched impact test piece of sintered metal materials. The test piece may be obtained directly by pressing and sintering or by machining a sintered part.
ISO 5754 applies to all sintered metals and alloys, with the exception of hardmetals. However, for certain materials (for example, materials with low porosity or materials with high ductility), it may be more appropriate to use a notched test piece which, in this case, will give results with less scatter. (In this case, refer to ISO 148‑1.)
NOTE For porous sintered materials, the results obtained from impact tests are not necessarily very accurate compared with results obtained from tests on solid metals.
-
Текущий статус: PublishedДата публикации: 2017-09
-
Версия: 2
-
Технический комитет: ISO/TC 119/SC 3 Sampling and testing methods for sintered metal materials (excluding hardmetals)
Приобрести данный стандарт
Формат | Язык | |
---|---|---|
std 1 40 | PDF + ePub | |
std 2 40 | Бумажный |
- CHF40
Жизненный цикл
-
Ранее
WithdrawnISO 5754:1978
-
Сейчас
PublishedISO 5754:2017
Стандарт, который пересматривается каждые 5 лет
Этап: 90.92 (Будет пересмотрено)-
00
Предварительная стадия
-
10
Стадия, связанная с внесением предложения
-
20
Подготовительная стадия
-
30
Стадия, связанная с подготовкой проекта комитета
-
40
Стадия, связанная с рассмотрением проекта международного стандарта
-
50
Стадия, на которой осуществляется принятие стандарта
-
60
Стадия, на которой осуществляется публикация
-
90
Стадия пересмотра
-
95
Стадия, на которой осуществляется отмена стандарта
-
00
-
Будет заменено
Under developmentISO/FDIS 5754
Появились вопросы?
Ознакомьтесь с FAQ
Часы работы:
Понедельник – пятница: 09:00-12:00, 14:00-17:00 (UTC+1)
Будьте в курсе актуальных новостей ИСО
Подписывайтесь на наши новости, обзоры, а также на информацию о продуктах.